Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® NY1820-BK1(PTFE) Lubricated, Heat Stabilized Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® NY1820-BK1(PTFE) Lubricated, Heat Stabilized Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lubricated, Heat Stabilized Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.020 - 0.024 cm/cm
0.020 - 0.024 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527-93
Elongation at Break 10 %
10 %
ISO 527-93
Flexural Strength 95.0 MPa
13800 psi
ISO 178-93
Flexural Modulus 2.80 GPa
406 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-93