Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Nucleated
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Lubricated, Nucleated, Unfilled Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm
0.017 - 0.019 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-93
Elongation at Break 30 %
30 %
ISO 527-93
Flexural Strength 80.0 MPa
11600 psi
ISO 178-93
Flexural Modulus 2.80 GPa
406 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Copyright © lookpolymers.com All Rights Reserved