Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral Reinforced, Toughened Grade Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183-87
Filler Content 32 %
32 %
Linear Mold Shrinkage, Flow 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527-93
Elongation at Break 15 %
15 %
ISO 527-93
Flexural Strength 80.0 MPa
11600 psi
ISO 178-93
Flexural Modulus 3.30 GPa
479 ksi
ISO 178-93
Izod Impact, Notched (ISO) 10.6 kJ/m²
5.04 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved