Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved surface appearance gradeAll information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527-93
Elongation at Break 2.0 %
2.0 %
ISO 527-93
Flexural Strength 190 MPa
27600 psi
ISO 178-93
Flexural Modulus 9.80 GPa
1420 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-93
Users viewing this material also viewed the following: