Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mineral Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 92.0 MPa
13300 psi
ISO 527-93
Elongation at Break 4.0 %
4.0 %
ISO 527-93
Flexural Strength 145 MPa
21000 psi
ISO 178-93
Flexural Modulus 6.10 GPa
885 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.90 kJ/m²
1.86 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ISO 75-93