Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GF33AO99 HR 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF33AO99 HR 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183-87
Filler Content 33 %
33 %
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
ISO 527-93
Elongation at Break 5.0 %
5.0 %
ISO 527-93
Flexural Strength 285 MPa
41300 psi
ISO 178-93
Flexural Modulus 9.75 GPa
1410 ksi
ISO 178-93
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-93
Flammability, UL94 HB

@Thickness 0.790 mm
HB

@Thickness 0.0311 in
Users viewing this material also viewed the following: