Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman EcoLon® MRGF1619-WBK1 Mineral and Glass Reinforced Recycled Nylon 66

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66 , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name EcoLon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman EcoLon® MRGF1619-WBK1 Mineral and Glass Reinforced Recycled Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Post Consumer Nylon Compound; WeatherableInformation provided by Wellman.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183-87
Filler Content 19 %
19 %
Linear Mold Shrinkage 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ISO 527-93
Elongation at Break 8.0 %
8.0 %
ISO 527-93
Flexural Strength 100 MPa
14500 psi
ISO 178-93
Flexural Modulus 3.70 GPa
537 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75-93
Copyright © lookpolymers.com All Rights Reserved