Wellman AquaClear® Ti844 PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Wellman
Trade Name AquaClear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman AquaClear® Ti844 PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AquaClearTI® 844 is a TPA-based polyethylene terephthalate resin made especially for use in the packaging applications. It’s a solid state copolymer resin with an intrinsic viscosity of 0.72. AquaClearTI® 844 may be used in contact with food in full compliance with the Federal Food, Drug, and Cosmetic Act and applicable food additive regulations including 21 CFR Section 177.1630. AquaClear does not contain antimony.Information provided by DAK Americas. Wellman is a subsidiary of DAK Americas.
Physical Properties Metric English Comments
Bulk Density 0.897 g/cc
0.0324 lb/in³
nominal
Viscosity Measurement 0.70 - 0.74
0.70 - 0.74
Intrinsic; BD-61201-1
Thermal Properties Metric English Comments
Melting Point >= 240 °C
>= 464 °F
BD-61305
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Chip Size 0.3-0.5 gm/20 chips
BD-61223
Color -5.0 - -1.0
b*, BD-66060
75-79
L*, BD-66060
Compounds <1 ppm
Acetaldehyde, measured on chip, BD-61301