| Category | Metal , Nonferrous Metal , Nickel Alloy |
| Manufacturer | Weartech |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.80 g/cc | 0.282 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell C | 54 - 62 | 54 - 62 | |
| Hardness, Vickers | 100 <br>@Treatment Temp. 760 °C |
100 <br>@Treatment Temp. 1400 °F |
|
| 250 <br>@Treatment Temp. 649 °C |
250 <br>@Treatment Temp. 1200 °F |
||
| 430 <br>@Treatment Temp. 538 °C |
430 <br>@Treatment Temp. 1000 °F |
||
| 540 <br>@Treatment Temp. 427 °C |
540 <br>@Treatment Temp. 800 °F |
||
| 750 <br>@Treatment Temp. 25.0 °C |
750 <br>@Treatment Temp. 77.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 14.6 µm/m-°C | 8.10 µin/in-°F | |
| Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
| Melting Point | <= 1040 °C | <= 1900 °F | |
| Liquidus | 1040 °C | 1900 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Boron, B | 3.0 % | 3.0 % | |
| Carbon, C | 0.70 % | 0.70 % | |
| Chromium, Cr | 14 % | 14 % | |
| Iron, Fe | 4.5 % | 4.5 % | |
| Nickel, Ni | 73.8 % | 73.8 % | |
| Silicon, Si | 4.0 % | 4.0 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Corrosion Resistance, Hydrochloric Acid Conc. 5.65% | >50 mils/year | RT |
| >50 mils/year | Boiling | |
| Corrosion Resistance, Nitric Acid Conc. 25-65% | >20 mils/year | RT |
| Corrosion Resistance, Sulfuric Acid Conc. 5-10% | >20 mils/year | RT |
| Relative Wear Performance | Cold Abrasion | Excellent |
| Corrosion | Good/Moderate | |
| Erosion | Good/Moderate | |
| Hot Abrasion | Good/Moderate | |
| Impact | Not Recommended | |
| Metal to Metal | Excellent |