Weartech International WT-12H Cobalt Hardfacing & Wear Resistant Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy
Manufacturer Weartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Weartech International WT-12H Cobalt Hardfacing & Wear Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: saw blades and tips, wood cutting toolsInformation provided by Weartech International
Mechanical Properties Metric English Comments
Hardness, Rockwell C 44 - 54
44 - 54
Component Elements Properties Metric English Comments
Carbon, C 1.7 %
1.7 %
Chromium, Cr 29 %
29 %
Cobalt, Co 53.8 - 59.8 %
53.8 - 59.8 %
Iron, Fe <= 3.0 %
<= 3.0 %
Nickel, Ni <= 3.0 %
<= 3.0 %
Silicon, Si 1.5 %
1.5 %
Tungsten, W 8.0 %
8.0 %