Material Notes:
Applications: for cobalt-free components in nuclear applications, valvesInformation provided by Weartech International, Norem is a registered trademark of Electric Power Research Institute
Mechanical Properties Metric English Comments
Hardness, Rockwell C 37 - 40
37 - 40
Component Elements Properties Metric English Comments
Carbon, C 1.1 %
1.1 %
Chromium, Cr 22 %
22 %
Iron, Fe 64.2 %
64.2 %
Manganese, Mn 3.7 %
3.7 %
Molybdenum, Mo 1.9 %
1.9 %
Nickel, Ni 4.5 %
4.5 %
Nitrogen, N <= 0.10 %
<= 0.10 %
Silicon, Si 2.5 %
2.5 %