Washington Penn PPH4CF1 Polypropylene, 10% Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn PPH4CF1 Polypropylene, 10% Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Wash tubs.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Melt Flow 13 - 15 g/10 min
13 - 15 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Flexural Yield Strength 31.0 MPa
4500 psi
ASTM D790
Flexural Modulus 1.60 GPa
232 ksi
Tangent; ASTM D790
Gardner Impact 11.0 J
8.11 ft-lb
ASTM D3029