Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Washington Penn PPC3MF1.5-Black Polypropylene, 15% Mica-Filled, Chemically-Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn PPC3MF1.5-Black Polypropylene, 15% Mica-Filled, Chemically-Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat Stabilized injection molding compound. Meets physical requirements for General Motors Spec. GMP.PP.024.Applications: HVAC duct and other various automotive applications.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
Melt Flow 7.0 g/10 min
7.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Flexural Yield Strength 44.0 MPa
6380 psi
ASTM D790
Flexural Modulus 1.60 GPa
232 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.500 J/cm

@Thickness 3.17 mm
0.937 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Users viewing this material also viewed the following: