Material Notes:
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array of colors.Information provided by Washington Penn Plastic Co.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Filler Content 10 %
10 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.8 MPa
5050 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.90 GPa
275 ksi
1% Secant; ASTM D790
2.07 GPa
300 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Gardner Impact 0.904 J

@Temperature 23.0 °C
0.667 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648