Material Notes:
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 16.0 MPa
2320 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.00500 GPa
0.725 ksi
ASTM D412
300% Modulus 0.0100 GPa
1.45 ksi
ASTM D412
Tear Strength 75.0 kN/m
428 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Processing Properties Metric English Comments
Processing Temperature 180 - 200 °C
356 - 392 °F