Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 54
54
ASTM D2240
Tensile Strength 29.0 MPa
4210 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.0100 GPa
1.45 ksi
ASTM D412
300% Modulus 0.0250 GPa
3.63 ksi
ASTM D412
Tear Strength 115 kN/m
656 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -30.0 °C
-22.0 °F
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F