Wall Colmonoy WALLEX 60 - Cobalt-Nickel Alloy

Category Metal , Metal Matrix Composite , Nonferrous Metal , Cobalt Alloy , Tungsten Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name WALLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy WALLEX 60 - Cobalt-Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Uses a cobalt-nickel matrix alloy to hold extremely hard tungsten-carbide particles. Primarily to protect surfaces against severe sliding abrasion. Finished by grinding.Method of Application: SpraywelderInformation provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 11.9 g/cc
0.430 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C >= 58
>= 58
Component Elements Properties Metric English Comments
Boron, B 2.3 %
2.3 %
Carbon, C 2.3 %
2.3 %
Chromium, Cr 12.35 %
12.35 %
Cobalt, Co 36.25 %
36.25 %
As Balance
Iron, Fe 0.65 %
0.65 %
Nickel, Ni 9.0 %
9.0 %
Silicon, Si 1.75 %
1.75 %
Tungsten, W 35.4 %
35.4 %
Processing Properties Metric English Comments
Processing Temperature 1110 °C
2030 °F
fusing temperature