Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wall Colmonoy COLMONOY® 228 Custom Formulated Nickel-Based Alloy For Glass

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLMONOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLMONOY® 228 Custom Formulated Nickel-Based Alloy For Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 8.46 g/cc
0.306 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28 - 33
28 - 33
Processing Properties Metric English Comments
Processing Temperature 929.4 °C
1705 °F
fusing temperature