Wall Colmonoy COLMONOY® 225 - Custom Formulated Nickel-Based Alloy For Glass

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLMONOY®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLMONOY® 225 - Custom Formulated Nickel-Based Alloy For Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description and Application: Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 8.59 g/cc
0.310 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 13 - 18
13 - 18
Processing Properties Metric English Comments
Processing Temperature 899 °C
1650 °F
fusing temperature