Material Notes:
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.850 g/cc
0.0253 - 0.0307 lb/in³
Powder Density; ISO 60
Density 1.70 g/cc
0.0614 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 - 85.0 MPa
8700 - 12300 psi
ISO 527
Elongation at Break 0.60 - 0.70 %
0.60 - 0.70 %
Tensile; ISO 527
1.3 - 1.5 %
1.3 - 1.5 %
Flexure; ISO 178
Tensile Modulus 12.5 - 14.5 GPa
1810 - 2100 ksi
ISO 527
Flexural Strength 140 - 180 MPa
20300 - 26100 psi
At Rupture; ISO 178
Flexural Modulus 11.0 - 14.0 GPa
1600 - 2030 ksi
ISO 178
Compressive Strength 240 - 280 MPa
34800 - 40600 psi
ISO 604
Charpy Impact Unnotched 0.800 - 1.10 J/cm²
3.81 - 5.24 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.250 - 0.400 J/cm²
1.19 - 1.90 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C

@Temperature 20.0 °C
22.2 - 27.8 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 170 - 180 °C
338 - 356 °F
ISO 75 Af
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
Shrinkage 0.050 - 0.15 %
0.050 - 0.15 %
Post Shrinkage; ISO 2577
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
Dry; IEC 167
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 243
Comparative Tracking Index 125 V
125 V
IEC 112
Descriptive Properties Value Comments
Color Black, Green
ISO type PF 2 C1
Main Filler Glass Fiber, Glass Bead, Graphite
Molding Method Compression, transfer, injection