Material Notes:
High heat extrusion crystalSuperior oriented polystyrene sheetFeatures: Low melt flowHigh molecular weightApplications: Foam applications such as egg cartons, meat trays and food serviceSuperior oriented polystyrene sheetInformation provided by Dax Resinas
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ISO 060
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Melt Flow 1.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ASTM D638
Tensile Modulus 3.24 GPa
470 ksi
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 3.24 GPa
470 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
@ 264 psi; ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB
HB