Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® 708 Polyetheretherketone (PEEK) Powder

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® 708 Polyetheretherketone (PEEK) Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VICOTE 708 and 709 grades are specially developed powder coatings (based on VICTREX HT™ polymer) with a higher Tg and melting point than the standard VICOTE products. VICOTE 708 and 709 grades deliver extended high temperature performance while offering all the key characteristics of standard VICOTE Coatings. Key features of VICOTE 708 and 709 grades include: Retention of mechanical and physical properties at temperatures 30°C higher than other 700 series coatings. Up to 3 times the wear resistance of standard 700 series coatings. Higher levels of fatigue performance. Higher creep modulus than standard 700 series coatings at 150°CVICOTE 708 and 709 grade powders are available in various average particle sizes from 10 – 50 microns. The powders are off-white in color and are available in various melt viscosities depending on the film thickness and level of melt flow required. Typical film thicknesses range from < 100 microns up to 500 microns. VICOTE 708 and 709 grades, like other non-coating grades of VICTREX HT polymer, are thermoplastic in nature and exhibit flow above the melt temperature. When processed using the correct guidelines, the coatings will exhibit the excellent properties that VICTREX HT polymer is renowned for. High continuous use temperature of 260°C Excellent wear abrasion and cut through resistance at these high temperatures Excellent chemical and radiation resistance Low level of extractables Hydrolysis resistant Inherently flame retardantAll information provided by Victrex.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Thermal Properties Metric English Comments
Melting Point 374 °C
705 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
Glass Transition Temp, Tg 157 °C
315 °F
DSC
UL RTI, Electrical 260 °C
500 °F
UL746B
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Users viewing this material also viewed the following: