Material Notes:
High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provided by VICTREX®
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Crystaline; ISO 1183
Viscosity 225000 cP

@Temperature 420 °C
225000 cP

@Temperature 788 °F
melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Tensile Modulus 4.20 GPa
609 ksi
ISO 527
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/U
Thermal Properties Metric English Comments
Glass Transition Temp, Tg >= 162 °C
>= 324 °F
Onset; ISO 11357
169 °C
336 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 410 - 420 °C
770 - 788 °F
Dry Time 3.00 hour

@Temperature 180 °C
3.00 hour

@Temperature 356 °F
6.00 hour

@Temperature 150 °C
6.00 hour

@Temperature 302 °F