Universal Wire Works Stellite 31 (AMS 5789) Filler Metal

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Stellite 31 (AMS 5789) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Haynes Stellite Alloy No. 31 is a cobalt base alloy having very good stress-rupture endurance and creep strength properties. No. 31 can be welded with the gas tungsten arc, gas metal arc and plasma welding processes.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.50 %
0.50 %
Chromium, Cr 26 %
26 %
Cobalt, Co >= 50.4 %
>= 50.4 %
As Remainder
Iron, Fe <= 2.0 %
<= 2.0 %
Manganese, Mn 1.0 %
1.0 %
Nickel, Ni 11 %
11 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.040 %
<= 0.040 %
Tungsten, W <= 8.0 %
<= 8.0 %