Universal Wire Works Multimet (N-155) (AMS 5794) Filler Metal

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Multimet (N-155) (AMS 5794) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multimet Alloy (N-155) can be welded using the gas tungsten arc and gas metal arc welding processes. Alloy N-155 has moderate resistance to stress up to 2000°F and excellent resistance to stress up to 1500°F. This alloy gains wide acceptance in the aircraft industry welding jet engine parts such as tailpipes, tail cones, afterburner parts, exhaust manifolds, turbine blades, buckets, nozzles and combustion chambers.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 21.5 %
21.5 %
Cobalt, Co 20 %
20 %
Iron, Fe >= 28.9 %
>= 28.9 %
As Remainder
Manganese, Mn 1.5 %
1.5 %
Molybdenum, Mo 3.0 %
3.0 %
Nb + Ta <= 1.25 %
<= 1.25 %
Nickel, Ni 20 %
20 %
Nitrogen, N <= 0.20 %
<= 0.20 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Tungsten, W 2.5 %
2.5 %