Material Notes:
Inconel Filler Metal 92 is a nickel base alloy designed especially for gas tungsten arc and gas metal arc welding of dissimilar combinations of high nickel alloys and austenitic and ferritic steels. Dissimilar applications of the alloy include joining Incoloy and Inconel alloys to carbon steels, stainless steels and Monel alloys; joining nickel base 200 and Monel alloys to stainless steels and joining stainless steels to carbon steels. Excellent results are obtained in joining 9% nickel steel to itself. Alloy 92 deposits are age hardenable.The mechanical properties listed as "annealed and aged" are minimum values after undergoing 1600°F/2 hr., A.C. + 1300°F/20 hr., A.C.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
As Welded
793 MPa
115000 psi
Annealed and Aged
Tensile Strength, Yield 276 MPa
40000 psi
As Welded
483 MPa
70000 psi
Annealed and Aged
Elongation at Break 10 %
10 %
Annealed and Aged
30 %
30 %
As Welded
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 15.5 %
15.5 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe 7.0 %
7.0 %
Manganese, Mn 2.4 %
2.4 %
Nickel, Ni 70 %
70 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.35 %
<= 0.35 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti 3.0 %
3.0 %