Universal Wire Works Hastelloy X (AMS 5798) Filler Metal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Hastelloy X (AMS 5798) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hastelloy Alloy X welding wire can be used with the gas tungsten arc, gas metal arc and plasma welding processes. Alloy X is used extensively in high temperature applications including engine tailpipes, turbine blades, afterburner components, nozzle vanes, cabin heaters and combustion liners.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Boron, B <= 0.010 %
<= 0.010 %
Carbon, C 0.10 %
0.10 %
Chromium, Cr 22 %
22 %
Cobalt, Co 1.5 %
1.5 %
Iron, Fe 19 %
19 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 9.0 %
9.0 %
Nickel, Ni >= 45.7 %
>= 45.7 %
As Remainder
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Tungsten, W 0.60 %
0.60 %