Universal Wire Works Greek Ascoloy (AMS 5817) Filler Metal

Category Metal , Ferrous Metal , Stainless Steel , Superalloy , Iron Base
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Greek Ascoloy (AMS 5817) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greek Ascoloy is primarily used for gas metal arc and gas tungsten arc welding of corrosion resistant steels of similar composition.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.15 %
<= 0.15 %
Carbon, C <= 0.20 %
<= 0.20 %
Chromium, Cr 13 %
13 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe >= 79.5 %
>= 79.5 %
As Remainder
Manganese, Mn <= 0.50 %
<= 0.50 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni 2.0 %
2.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.030 %
<= 0.030 %
Tin, Sn <= 0.050 %
<= 0.050 %
Tungsten, W 3.0 %
3.0 %