Universal Wire Works ER316LSi Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER316LSi Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This filler metal is the same as the 316L, except for the silicon content. The additional silicon improves the washing and wetting behavior of the weld metal. This feature reduces the finishing costs of welds particularly on thin base metals.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.00 - 0.030 %
0.00 - 0.030 %
Chromium, Cr 19 %
19 %
Iron, Fe 69.5 - 69.5 %
69.5 - 69.5 %
As Remainder
Molybdenum, Mo 2.5 %
2.5 %
Nickel, Ni 9.0 %
9.0 %