Universal Wire Works ER309L Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER309L Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This alloy is the same as ER309, except for the carbon content. Low (0.03% maximum) carbon in this filler metal reduces the possibility of intergranular carbine precipitation thus increases the resistance to intergranular corrosion without the use of stabilizers such as columbium titanium. It should be noted that at elevated temperatures the 309L deposit is not as strong as the stabilized grades or the standard ER309.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.00 - 0.030 %
0.00 - 0.030 %
Chromium, Cr 25 %
25 %
Iron, Fe 63 - 63 %
63 - 63 %
As Remainder
Nickel, Ni 12 %
12 %