Universal Wire Works ER308H Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER308H Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This filler metal is the same as ER308, except that the allowable carbon content has been restricted to the higher portion of the 308 range. Carbon content in the range of 0.04-0.08 provides higher strength. ER308H is used for welding 304H base metal.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.040 - 0.080 %
0.040 - 0.080 %
Chromium, Cr 19 %
19 %
Iron, Fe 71.9 - 72 %
71.9 - 72 %
As Remainder
Nickel, Ni 9.0 %
9.0 %