Universal Wire Works ER219 Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER219 Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Filler metals of this classification are most often used to weld UNS 21900 base metals. This alloy is a nitrogen-strengthened austenitic stainless steel exhibiting high strength and good toughness over a wide range of temperatures. Deposited weld metal is not subject to carbide precipitation due to the Nitrogen alloying which inhibits carbide precipitation in the weld zone.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Chromium, Cr 21 %
21 %
Iron, Fe 63.8 %
63.8 %
As Remainder
Manganese, Mn 9.0 %
9.0 %
Nickel, Ni 6.0 %
6.0 %
Nitrogen, N 0.25 %
0.25 %