Material Notes:
Alloy 71T1 is an all position, flux-cored electrode which is intended for the single and multiple pass welding of carbon and certain low alloy steels where a minimum tensile strength of 70,000 psi is required. Gas shielding can be (100% CO2) or (75% Ar / 25% CO2). This alloy is an excellent choice for general purpose, flux cored welding on steels, such as structural steel, farm machinery, construction equipment and general steel fabrications.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 571 MPa
82800 psi
Tensile Strength, Yield 490 MPa
71000 psi
Elongation at Break 25 %
25 %
Charpy Impact 78.6 J

@Temperature -17.8 °C
58.0 ft-lb

@Temperature 0.000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Iron, Fe 98.2 %
98.2 %
As Remainder
Manganese, Mn 1.0 %
1.0 %
Phosphorous, P 0.0080 %
0.0080 %
Silicon, Si 0.74 %
0.74 %
Sulfur, S 0.015 %
0.015 %