Universal Wire Works 99 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 99 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal nickel alloy 99 is used for arc welding cast iron to itself, low alloy steels and carbon steels. Alloy 99 is used in those applications that require maximum mach inability or where thin sections of casting are encountered. Alloy 99 can be used in all positions with either AC or DCRP.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Copper, Cu 0.10 %
0.10 %
Iron, Fe 3.0 %
3.0 %
Manganese, Mn 0.20 %
0.20 %
Nickel, Ni 95 %
95 %
Silicon, Si 0.70 %
0.70 %
Sulfur, S 0.0050 %
0.0050 %