Universal Wire Works 82 (AMS 5836) Filler Metal

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 82 (AMS 5836) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 82 is a corrosion and heat resistant alloy used extensively for gas tungsten arc and gas metal arc welding of parts fabricated from high nickel alloys or combination of such alloys and corrosion resistant or plain carbon steels.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 20 %
20 %
Cobalt, Co <= 0.12 %
<= 0.12 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn <= 3.0 %
<= 3.0 %
Nickel, Ni 69 %
69 %
Niobium, Nb (Columbium, Cb) 2.5 %
2.5 %
Other, total <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.015 %
<= 0.015 %
Tantalum, Ta <= 0.30 %
<= 0.30 %
Titanium, Ti <= 0.75 %
<= 0.75 %