Material Notes:
Alloy 60 is used for Gas Metal Arc Welding (GMAW), Gas Tungsten Arc Welding (GTAW), and Submerged Arc Welding (SMA) of Monel type alloys 400 and 404, as well as overlaying on steel. When GMAW or MIG welding overlays on steel a first pass of Alloy 61 is recommended. When using the submerged arc process with a flux, a layer of Alloy 61 is not necessary. Alloy 60 dissimilar metal welding applications include: joining Monel type alloys and nickel 200 to copper and copper-nickel alloys or Monel type alloys to nickel 200.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 483 MPa
70000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.25 %
<= 1.25 %
Carbon, C <= 0.015 %
<= 0.015 %
Copper, Cu >= 18.5 %
>= 18.5 %
As Remainder
Iron, Fe <= 2.5 %
<= 2.5 %
Manganese, Mn <= 4.0 %
<= 4.0 %
Nickel, Ni 62 - 69 %
62 - 69 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Silicon, Si <= 1.25 %
<= 1.25 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti 1.5 - 3.0 %
1.5 - 3.0 %