Alloy 4643 is used as a filler metal for GTAW of heavy sections of aluminum alloys of similar composition to produce joints having inherently low dilution ratio of base metal to weld metal and where the weldment may require heat treatment.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Aluminum, Al >= 95 %
>= 95 %
As Remainder
Beryllium, Be 0.00040 %
0.00040 %
Copper, Cu 0.050 %
0.050 %
Iron, Fe 0.40 %
0.40 %
Manganese, Mn 0.20 %
0.20 %
Other, each <= 0.050 %
<= 0.050 %
Other, total <= 0.15 %
<= 0.15 %
Silicon, Si 4.0 %
4.0 %
Titanium, Ti 0.080 %
0.080 %
Zinc, Zn 0.050 %
0.050 %