Universal Wire Works 310 Cb Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 310 Cb Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 310 Cb electrodes are the same as the 310 electrodes except for the addition of columbium and the reduction in the carbon content. This alloy is especially useful in the welding of types 304, 309, 310, 316, 321, and 347. Universal 310 Cb is also used for joining columbium stabilized stainless steel to mild or carbon steels.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 662 MPa
96000 psi
Elongation at Break 33 %
33 %
Component Elements Properties Metric English Comments
Carbon, C 0.11 %
0.11 %
Chromium, Cr 26.1 %
26.1 %
Iron, Fe 49.5 %
49.5 %
As Remainder
Manganese, Mn 1.95 %
1.95 %
Nickel, Ni 20.9 %
20.9 %
Niobium, Nb (Columbium, Cb) 0.90 %
0.90 %
Silicon, Si 0.50 %
0.50 %