Universal Wire Works 309 Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 309 Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 309 electrodes are used for the welding of heat resisting type 309 stainless steel. Deposits retain strength and oxidation resistance up to 2000 degrees F. Typical applications include furnace parts, kiln linings, and heat treat baskets. Alloy 309 is excellent for welding AISI types 405, 410, 430, 442, and 446 when preheat and postweld heat treatment is not practical. Alloy 309 is also used for welding the clad side of stainless clad steels and for joining mild or carbon steels to stainless steel.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 600 MPa
87000 psi
Elongation at Break 40 %
40 %
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 23.4 %
23.4 %
Iron, Fe 61 %
61 %
As Remainder
Manganese, Mn 1.8 %
1.8 %
Nickel, Ni 13.1 %
13.1 %
Silicon, Si 0.60 %
0.60 %