Universal Wire Works 17-7 (AMS 5824) Filler Metal

Category Metal , Ferrous Metal , Stainless Steel , Precipitation Hardening Stainless
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 17-7 (AMS 5824) Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 17-7PH is a precipitation-hardening filler metal designed for gas tungsten arc and gas metal arc welding of precipitation-hardening, corrosion resistant steels of similar composition where the weld area is required to have comparable strength and corrosion resistance to those of parent metal.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Aluminum, Al 1.0 %
1.0 %
Carbon, C <= 0.090 %
<= 0.090 %
Chromium, Cr 17 %
17 %
Iron, Fe 75 %
75 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 7.0 %
7.0 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.025 %
<= 0.025 %