Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works 122 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 122 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 122 is used for welding of nickel-chromium-molybdenum alloys as well as for overlay cladding on carbon, low alloy, or stainless steels. Alloy 122 is often used on dissimilar joints between nickel-chromium-molybdenum alloys and stainless, carbon, or low alloy steels. Alloy 122 is used for welding base metals under ASTM F574, B619, B622, and B626. This alloy offers excellent corrosion resistance in oxidizing as well as reducing media in a wide variety of chemical process environments. Alloy 122 exhibits superior resistance to stress corrosion, cracking, pitting and crevice corrosion.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 786 MPa
114000 psi
Tensile Strength, Yield 538 MPa
78000 psi
Elongation at Break 36 %
36 %
Component Elements Properties Metric English Comments
Carbon, C 0.014 %
0.014 %
Chromium, Cr 21.2 %
21.2 %
Iron, Fe 3.9 %
3.9 %
Manganese, Mn 0.35 %
0.35 %
Molybdenum, Mo 13.1 %
13.1 %
Nickel, Ni 58 %
58 %
As Remainder
Phosphorous, P 0.012 %
0.012 %
Silicon, Si 0.16 %
0.16 %
Sulfur, S 0.0050 %
0.0050 %
Tungsten, W 3.3 %
3.3 %
Users viewing this material also viewed the following: