Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.20 mm
0.0080 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Thickness 3.20 mm
0.010 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength at Break 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Strength 50.0 MPa
7250 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Compressive Strength 60.0 MPa
8700 psi
ASTM D362
Shear Strength 48.0 MPa
6960 psi
ASTM D732
Izod Impact, Notched 2.50 J/cm
4.68 ft-lb/in
ASTM D256