Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Unitika
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika E-RUNG60 Ultra high-rigidity PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultra high-rigidityInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 230 MPa
33400 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 330 MPa
47900 psi
ASTM D790
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Izod Impact, Notched 1.75 J/cm
3.28 ft-lb/in
ASTM D256