Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 60% Glass Fiber Filled
Manufacturer Unitika
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika E-RUNG60 PA66, 60% Glass Fiber Reinforced, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.70 %
0.70 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.20 mm
0.0010 in/in

@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0030 cm/cm

@Thickness 3.20 mm
0.0030 in/in

@Thickness 0.126 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa
31200 psi
ISO 527-1/-2
Elongation at Break 2.3 %
2.3 %
ISO 527-1/-2
Tensile Modulus 15.0 GPa
2180 ksi
ISO 527-1/-2
Flexural Strength 320 MPa
46400 psi
ISO 178
Flexural Modulus 14.7 GPa
2130 ksi
ISO 178
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179-1
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-2