Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant
Manufacturer Unitika
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.2 %
1.2 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.20 mm
0.0040 in/in

@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Thickness 3.20 mm
0.0080 in/in

@Thickness 0.126 in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ISO 2039
Tensile Strength at Break 87.0 MPa
12600 psi
ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/-2
Tensile Modulus 5.10 GPa
740 ksi
ISO 527-1/-2
Flexural Strength 120 MPa
17400 psi
ISO 178
Flexural Modulus 4.30 GPa
624 ksi
ISO 178
Charpy Impact Unnotched 5.60 J/cm²
26.6 ft-lb/in²
ISO 179-1
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-2
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in