Unitika AX-1500W Conditioned

Category Polymer , Thermoplastic , Polyarylate
Manufacturer Unitika
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika AX-1500W Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at display devices Chemical resistanceInformation provided by Unitika Ltd.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149
Dissipation Factor 0.040

@Frequency 1.00e+6 Hz
0.040

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 80 sec
80 sec
ASTM D495
Processing Properties Metric English Comments
Rear Barrel Temperature 200 - 220 °C
392 - 428 °F
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Nozzle Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
actual surface temp
Drying Temperature 100 °C
212 °F
Dry Time 10.0 - 24.0 hour
10.0 - 24.0 hour
Back Pressure 0.490 - 1.47 MPa
71.1 - 213 psi
gage pressure