Material Notes:
Made for blow molding, tubular film and special applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ISO 1183
ESCR 100% Igepal® >= 350 hour

@Temperature 50.0 °C
>= 350 hour

@Temperature 122 °F
ASTM D1693
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ISO 868
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Flexural Modulus 0.600 GPa
87.0 ksi
ISO 178
Charpy Impact, Notched 0.140 J/cm²

@Temperature 23.0 °C
0.666 ft-lb/in²

@Temperature 73.4 °F
ISO 179
0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F
ISO 306