Unipetrol Iso Butanol Synthetic

Category Fluid , Solvent
Manufacturer Unipetrol RPA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol Iso Butanol Synthetic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isobutanol is produced by propylene oxonation and by subsequent hydrogenation of the obtained isobutyraldehyde. It is a transparent, colourless, flammable liquid of a characteristic odour.Isobutanol is classified according to EC Directives as a hazardous substance.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.800 - 0.804 g/cc

@Temperature 20.0 °C
0.0289 - 0.0290 lb/in³

@Temperature 68.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Component Elements Properties Metric English Comments
Free Water <= 0.070 %
<= 0.070 %
Descriptive Properties Value Comments
Acetic Acid wt %, max 0.001
Carbonyls (as butyraldehyde), max 0.04
Isobutanol, min 99.2