Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct Single-Layer System Insulation

Category Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name FyreWrap®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct Single-Layer System Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unifrax's FyreWrap ™ 1.5 Duct Insulation is a single-layer flexible enclosure for 1- and 2-hour fire-rated commercial kitchen grease ducts and hazardous exhaust ducts including chemical fume ducts. This slim, compact design offers the lightest system available and results in significant weight, space and labor savings when compared to traditional fire-rated shafts or competitive wrap systems. The system was tested per UL 1978 and complies with pre-2006 editions of the International Mechanical Code (IMC). FyreWrap 1.5 provides the following features:Zero clearance to combustibles at all locations on wrap1- and 2-hour fire endurance ratingAlternate to fire-rated shaft enclosureSaves weight, space, laborThinnest, lightest system availableHigh-temperature, biosoluble insulationGREENGUARD listed for Microbial ResistanceProduct ComponentsCore Material: FyreWrap 1.5 incorporates Insulfrax Thermal Insulation as its core materail. Insulfrax is a high-temperature insulation made from a calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket product form.Encapsulating Material: The core insulation blanket is completely encapsulated in an aluminum foil fiberglass reinforced scrim covering. This scrim provides additional handling strength as well as protection from grease and moisture absorption and tearing.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.0961 g/cc
0.00347 lb/in³
Nominal
Thickness 38100 microns
1500 mil