Unifrax FyreWrap® Cable Insulation

Category Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name FyreWrap®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax FyreWrap® Cable Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unifrax's FyreWrap® Cable Insulation is a thin, flexible, insulation wrap designed to provide a fire-protective enclosure around cable trays and conduit. The FyreWrap system ensures electrical circuit integrity during exposure to an external hydrocarbon fire, permitting continued operation or controlled shutdown of critical equipment during emergency conditions. This system is FM Global approved and meets ASTM E-1725 "Fire Tests of Fire-Resistive Barrier Systems for Electrical System Components," the newest industry standard, requiring the highest level of performance for trays with zero to full cable loading. The system also meets ASTM E-1529 and provides circuit integrity ratings. FyreWrap complies with API and ExxonMobil specifications on fireproofing for petroleum and petrochemical processing plants.Product ComponentsCore Material: FyreWrap Cable Insulation products incorporate Insulfrax® Thermal Insulation as its core material. Insulfrax is a high-temperature insulation made from calcia, magnesia, silica chemistry designed to enhance biosolubility. It provides excellent insulation in a noncombustible blanket form.Encapsulating Material: The core insulation is completely encapsulated in an aluminum foil, fiberglass-reinforced scrim covering. This scrim provides additional handling strength as well as protection from tearing and moisture absorption. For outdoor installations, additional weather protection should be considered.Typical System PropertiesFM Global Approved - Wrap for Grouped Electrical CablesAPI 2218 "Fireproofing Practices in Petroleum and Petrochemical Processing Plants" - compliesExxonMobil GP14-03-01 "Fireproofing" Specification - compliesFire Exposure - Hydrocarbon Fire per ASTM E-1529Circuit Integrity - per ASTM E-1529Temperature Integrity - per ASTM E-1725Cable Loading - Empty to Fully Loaded TraysFire Rating - 30, 45, 60 minutesASTM E-84 Surface Burning Characteristics: (1) Unfaced Core: Flame/Smoke Rating = Zero, (2) FyreWrap: Flame/Smoke Rating < 25-50Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.128 g/cc
0.00463 lb/in³
Thickness 38100 microns
1500 mil
50800 microns
2000 mil